Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 0.157 kV/mm @Thickness 3.17 mm |
4.00 kV/in @Thickness 0.125 in |
Unconditioned; ASTM D149 |
Garlock 8314 EPDM Sheet Rubber Gasketing Ethylene Propylene Diene Monomer (EPDM)Resists weathering, ozone, and UV exposure.Information provided by Garlock Rubber Technologies |
|||
Dielectric Strength | 0.157 kV/mm @Thickness 3.17 mm |
4.00 kV/in @Thickness 0.125 in |
Unconditioned; ASTM D149 |
Garlock 9122 Nitrile Sheet Rubber Gasketing Nitrile (NBR)Superior resistance to aliphatic hydrocarbons, such as oil, fuels, and many types of solvents.Information provided by Garlock Rubber Technologies |