Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 0.122 - 20.0 kV/mm | 3.10 - 508 kV/in | Average value: 16.3 kV/mm Grade Count:8 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |