Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746 |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 401 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | PLC code 1; UL 746A |
SABIC Innovative Plastics Valox® 735 PBT 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Valox® 735 PBT+PET 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA 30% Glass Reinforced PPE+PA Alloy. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific) GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min @Thickness 1.50 mm |
0.394 - 1.00 in/min @Thickness 0.0591 in |
UL Rating PLC 1 (10-25.4 mm/min.) |
Covestro Makrolon® 3105 Polycarbonate Injection molding and extrusion grade with high viscosity, with easy mold release.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and official.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | Average value: 17.7 mm/min Grade Count:5 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.1 - 25.4 mm/min | 0.398 - 1.00 in/min | UL 746 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 402 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t.. |