Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 915R PC (Asia Pacific) Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 915RP PC (Asia Pacific) Lexan* 915RP Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.05 mm |
0.000 - 0.394 in/min @Thickness 0.120 in |
UL PLC 0 (0-10 mm/min) |
Resinoid 1340 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | Average value: 5.00 mm/min Grade Count:4 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.00 mm |
0.000 - 0.394 in/min @Thickness 0.118 in |
BK |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.50 mm |
0.000 - 0.394 in/min @Thickness 0.0591 in |
BK |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL746A |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL746A |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2312 PEI 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2312 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.60 mm |
0.000 - 0.394 in/min @Thickness 0.0630 in |
UL PLC 0 (0-10 mm/min) |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.05 mm |
0.000 - 0.394 in/min @Thickness 0.120 in |
UL PLC 0 (0-10 mm/min) |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.47 mm |
0.000 - 0.394 in/min @Thickness 0.0579 in |
UL PLC 0 (0-10 mm/min) |
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.57 mm |
0.000 - 0.394 in/min @Thickness 0.0618 in |
UL PLC 0 (0-10 mm/min) |
Sumitomo Bakelite North America RX® 3-1-525F-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.70 mm |
0.000 - 0.394 in/min @Thickness 0.0669 in |
UL PLC 0 (0-10 mm/min) |
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |