Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 104 PC (Asia Pacific) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 124R PC UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 131R PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 223 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific) 10.5 MFR. Improved flame retardance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® LS2 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 144 PC (Asia Pacific) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® HP4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL Rating PLC 2 (25.4-80 mm/min) |
LG Chemical MI-770 MIPS |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific) Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 1100F PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant. UL94 V0, V2 and 5VA listing. Effective June 2007, this grade will no longer be supported with biocompa.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 1110F PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 listing. UL94 V0 and 5VA listing. Effective June 2007, this grade will no longer be supported w.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2200R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | PLC code 2; UL 746A |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2110R PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min @Thickness 1.50 mm |
1.00 - 3.15 in/min @Thickness 0.0591 in |
UL Rating PLC 2 (25.4-80 mm/min.) |
Covestro Makrolon® 2805 Polycarbonate, Injection Grade Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.5 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.5 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 143R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
SABIC Innovative Plastics ULTEM 2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |