Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 330 mm/min | 0.000 - 13.0 in/min | Average value: 116 mm/min Grade Count:3 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |