Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 208 mm/min

@Thickness 1.60 mm
8.19 in/min

@Thickness 0.0630 in
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
High Voltage Arc-Tracking Rate, HVTR 208 mm/min

@Thickness 1.60 mm
8.19 in/min

@Thickness 0.0630 in
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..