Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | PLC code 1; UL 746A |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® EX58 ABS High impact ABS for sheet extrusion and blow molding applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | Average value: 15.8 mm/min Grade Count:4 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 50.0 mm/min | 0.394 - 1.97 in/min | Average value: 32.7 mm/min Grade Count:4 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS High impact and ductility at 73F and -20F. For thin-wall applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min @Thickness 3.00 mm |
0.394 - 1.00 in/min @Thickness 0.118 in |
BN, BK |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min | <= 0.394 in/min | UL Rating PLC 0 (0-10 mm/min) |
LG Chemical 65IH HIPS High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 25SPI GPPS High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 401 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl.. |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min | <= 0.394 in/min | UL Rating PLC 0 (0-10 mm/min) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min | <= 0.394 in/min | UL Rating PLC 0 (0-10 mm/min) |
LG Chemical 95HC SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min | <= 0.394 in/min | UL Rating PLC 0 (0-10 mm/min) |
LG Chemical SG-950 Alphalac Polystyrene High strength, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electr.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | PLC code 1; UL 746A |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min @Thickness 3.00 mm |
<= 0.394 in/min @Thickness 0.118 in |
UL Rating PLC 0 (<10 mm/min.) |
Covestro Makrolon® 2407 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |