Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943AR PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® FL920 PC Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® 151 PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 945U PC (Asia Pacific) Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 953A PC (Asia Pacific) Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 0.750 mm |
30 - 60 arcs @Thickness 0.0295 in |
NC |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 0.810 mm |
30 - 60 arcs @Thickness 0.0319 in |
ALL |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.50 mm |
30 - 60 arcs @Thickness 0.0591 in |
BN, BK |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.50 mm |
30 - 60 arcs @Thickness 0.0591 in |
|
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
|
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Noryl PX5622 PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL SPN410 PPE+PS Improved productivity. 210F (99C) DTUL. UL94 HB rated. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | |
Sylvin Technologies 916V0 Black PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Noryl N190HX PPE+PS High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL PN235 PPE+PS Plating grade, primarily automotive applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL PN235 PPE+PS (Asia Pacific) Plating grade, primarily automotive applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4020 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL BN31 PPE+PS Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.50 mm |
30 - 60 arcs @Thickness 0.0591 in |
UL Rating PLC 2 (30-60 arcs) |
Covestro Makrolon® 6255 Polycarbonate, Flame Retardant, High Productivity, Mold Release Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.50 mm |
30 - 60 arcs @Thickness 0.0591 in |
UL Rating PLC 2 (30-60 arcs) |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |