Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycolac® MGABS01 ABS Injection molding ABS. High impact, high gloss, good flow. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® EHA PC+ABS (Asia Pacific) PC+ABS. Electroplateable. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® LUX9610 PC (Asia Pacific) Lexan LUX9610 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS High impact and ductility at 73F and -20F. For thin-wall applications. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 3.35 mm |
15 - 30 sec @Thickness 0.132 in |
UL Rating PLC 3 (15-30 sec) |
Ineos ABS Centrex® 401 AES Extrusion
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical MI-770 MIPS |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific) 6.5% GR PBT, UL94 V-0/5V. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics NORYL PX1543 PPE+PS |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
SABIC Innovative Plastics Valox® 451E PBT 20% GR. Easy flow version of VALOX 451. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 3.00 mm |
15 - 30 sec @Thickness 0.118 in |
UL Rating PLC 3 (15-30 sec) |
Covestro Makrolon® 2407 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
UL Rating PLC 3 (15-30 sec) |
Covestro Makrolon® 2607 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially a.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |