Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 500R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 34.5 sec Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Hot Wire Ignition, HWI | 0.000 - 120 sec | 0.000 - 120 sec | Average value: 54.3 sec Grade Count:14 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® FL920 PC (Asia Pacific) Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
Hot Wire Ignition, HWI | 30.0 - 120 sec | 30.0 - 120 sec | Average value: 85.0 sec Grade Count:3 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 6.00 mm |
60 - 120 sec @Thickness 0.236 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **) Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially.. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 40.8 sec Grade Count:4 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific) 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1000RV PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1100F PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June 2007, this grade will no longer be supported with biocompati.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2210R PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 2212 PEI (Asia Pacific) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 553 PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 553U PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific) 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1017 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4101 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 536 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |