Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 3413HF PC 30% glass reinforced, high flow PC. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC 1 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific) 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Prevex BJAX PPE+PS Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2210R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 2212 PEI 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem MD130A PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific) 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4011 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4020 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC 1; UL 746 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**) Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad.. |