Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 34.5 sec Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 70.9 sec Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 25.9 sec Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 24.1 sec Grade Count:15 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Hot Wire Ignition, HWI | 7.00 - 30.0 sec | 7.00 - 30.0 sec | Average value: 16.8 sec Grade Count:4 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Hot Wire Ignition, HWI | 7.00 - 30.0 sec | 7.00 - 30.0 sec | Average value: 16.8 sec Grade Count:4 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 85.0 sec Grade Count:4 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 20.7 sec Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 20.1 sec Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 20.9 sec Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 33.6 sec Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Hot Wire Ignition, HWI | 7.00 - 120 sec | 7.00 - 120 sec | Average value: 40.8 sec Grade Count:4 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Hot Wire Ignition, HWI | 7.00 - 59.0 sec | 7.00 - 59.0 sec | Average value: 14.8 sec Grade Count:14 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 20.9 sec Grade Count:3 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 26.8 sec Grade Count:4 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Hot Wire Ignition, HWI | 7.00 - 30.0 sec | 7.00 - 30.0 sec | Average value: 21.1 sec Grade Count:5 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |