Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 500R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC 1 |
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1100F PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June 2007, this grade will no longer be supported with biocompati.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem 1100FV PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 1110F PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be supported wit.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2110 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2300 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific) 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1017 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | PLC code 1; UL 746A |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 1 (60-120 sec) |
Covestro Makrolon® 6485 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was .. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |