Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 2.0 sec @Thickness >=1.50 mm |
2.0 sec @Thickness >=0.0591 in |
ASTM D3874-88 |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Hot Wire Ignition, HWI | 2.0 sec @Thickness >=1.50 mm |
2.0 sec @Thickness >=0.0591 in |
ASTM D3874-88 |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Hot Wire Ignition, HWI | 2.0 sec @Thickness >=1.50 mm |
2.0 sec @Thickness >=0.0591 in |
ASTM D3874-88 |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Hot Wire Ignition, HWI | 2.0 sec @Thickness >=1.50 mm |
2.0 sec @Thickness >=0.0591 in |
ASTM D3874-88 |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Hot Wire Ignition, HWI | 2.0 sec @Thickness >=1.50 mm |
2.0 sec @Thickness >=0.0591 in |
ASTM D3874-88 |
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Hot Wire Ignition, HWI | 2.0 sec @Thickness >=1.50 mm |
2.0 sec @Thickness >=0.0591 in |
ASTM D3874-88 |
BASF Ultramid® B3UG4 LS Grey22985 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |