Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 3414R PC 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Hot Wire Ignition, HWI | 120 sec | 120 sec | Average value: 120 sec Grade Count:4 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
ALL |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746A |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL PX9406 PPE+PS Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1530 compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM ATX200R PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. RoHS compliant. UL94 V0 Listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5011 PEI Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) 19.5% glass reinforced PBT. High flow, flame retardant. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific) 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | PLC code 0; UL 746A |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH7010 PPE+PS Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL PX1265 PPE+PS (Asia Pacific) Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific) GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 0.860 mm |
>= 120 sec @Thickness 0.0339 in |
PLC 0 |
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |