Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 95.0 °C | 203 °F | |
PPT FP95 Fully Sintered Ferrite Powder Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu.. |
|||
Curie Temperature | 95.0 °C | 203 °F | |
PPT BP2000 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or.. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i.. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 o.. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Curie Temperature | <= 95.0 °C | <= 203 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Curie Temperature | 95.0 - 105 °C | 203 - 221 °F | |
Goodfellow Ni-Mn-Ga Magnetic Shape Memory Alloy (MSM) Ni50Mn28.5Ga21.5 single crystal. The magnetic shape memory phenomenon is produced by magnetic-field-induced rearrangement of (ferromagnetic) twinned martensite microstructure accompanied by a large .. |