Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | -6.67 - 10.0 °C | 20.0 - 50.0 °F | |
Carlson C 400 Nickel-Copper Alloy General DescriptionCarlson Alloy C 400 is a nickel-copper alloy which provides an excellent combination of high strength, ductility, good weldability, and resistance to corrosion over a wide range o.. |