Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 750 °C | 1380 °F | |
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Curie Temperature | 750 °C | 1380 °F | |
Carpenter Chrome Core® 8 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-20A Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-26A Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-26B Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-28B Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-30B Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Carpenter Chrome Core® 8-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-28H Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-32 Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-22A Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-26H Samarium Cobalt Magnetic Material |
|||
Curie Temperature | 750 °C | 1380 °F | |
Carpenter Chrome Core® 12-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Curie Temperature | 750 °C | 1380 °F | |
Alliance S-22B Samarium Cobalt Magnetic Material |