Polymer Property : Curie Temperature = 320 °C Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature 320 °C
608 °F
Piezo Kinetics 804 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp..
Curie Temperature 320 °C
608 °F
Tc
CeramTec Sonox® P88 Piezoceramic
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics ..
Curie Temperature 320 °C
608 °F
Alliance N-35M Neodymium Iron Boron Magnetic Material
Curie Temperature 320 °C
608 °F
Alliance N-40M Neodymium Iron Boron Magnetic Material
Curie Temperature 320 °C
608 °F
Alliance N-42M Neodymium Iron Boron Magnetic Material
Curie Temperature 320 °C
608 °F
Alliance N-45M Neodymium Iron Boron Magnetic Material
Curie Temperature 320 °C
608 °F
Alliance N-38M Neodymium Iron Boron Magnetic Material
Curie Temperature 320 °C
608 °F
Alliance N-33M Neodymium Iron Boron Magnetic Material