Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | -124.4 °C | -191.9 °F | |
Carlson C 600 Nickel-Chromium-Iron Alloy Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c.. |
|||
Curie Temperature | -124.4 °C | -191.9 °F | |
Carlson C 600ESR Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell.. |