Polymer Property : Curie Temperature = -112 °C Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 0% Cold Worked, Not Aged
0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes ..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 10% Cold Worked
10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 15% Cold Worked, Aged
15% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 20% Cold Worked
20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 25% Cold Worked, Aged
25% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 30% Cold Worked, Aged
30% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 50% Cold Worked
50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Curie Temperature -112 °C
-170 °F
Special Metals INCONEL® Alloy 718
Developed in the early 1960's, IN718 is still considered the material of choice for the majority of aircraft engine components with service temperatures below 1200°F (650°C). Inconel 718 is a..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 10% Cold Worked, Aged
10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 15% Cold Worked
15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 30% Cold Worked
30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 5% Cold Worked
5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 5% Cold Worked, Aged
5% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Inte..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 50% Cold Worked, Aged
50% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 20% Cold Worked, Aged
20% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Curie Temperature -112 °C
-170 °F
HP Alloys Alloy 718, 25% Cold Worked
25% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..