Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 11500 Gauss | 11500 Gauss | |
Alliance N-33 Neodymium Iron Boron Magnetic Material |
|||
Magnetic Remanence, Br | 11500 Gauss | 11500 Gauss | |
Alliance N-33H Neodymium Iron Boron Magnetic Material |
|||
Magnetic Remanence, Br | 11500 Gauss | 11500 Gauss | |
Alliance N-33SH Neodymium Iron Boron Magnetic Material |
|||
Magnetic Remanence, Br | 11500 Gauss | 11500 Gauss | |
Alliance N-33UH Neodymium Iron Boron Magnetic Material |
|||
Magnetic Remanence, Br | 11500 Gauss | 11500 Gauss | |
Alliance S-32 Samarium Cobalt Magnetic Material |
|||
Magnetic Remanence, Br | 11500 Gauss | 11500 Gauss | |
Alliance N-33M Neodymium Iron Boron Magnetic Material |