Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 9000 - 9600 Gauss | 9000 - 9600 Gauss | |
Ceradyne SEMICORE® S2-17B MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |