Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 11000 Gauss | 11000 Gauss | |
Alliance N-30EH Neodymium Iron Boron Magnetic Material |
|||
Magnetic Remanence, Br | 11000 Gauss | 11000 Gauss | |
Alliance N-30UH Neodymium Iron Boron Magnetic Material |
|||
Magnetic Remanence, Br | 11000 Gauss | 11000 Gauss | |
Alliance S-30A Samarium Cobalt Magnetic Material |