Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 10000 Oe | 10000 Oe | |
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
Magnetic Coercive Force, Hc | 10000 Oe | 10000 Oe | |
Alliance S-28B Samarium Cobalt Magnetic Material |
|||
Magnetic Coercive Force, Hc | 10000 Oe | 10000 Oe | |
Alliance S-28H Samarium Cobalt Magnetic Material |
|||
Magnetic Coercive Force, Hc | 10000 Oe | 10000 Oe | |
Alliance S-32 Samarium Cobalt Magnetic Material |