Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 16000 Oe | 16000 Oe | Intrinsic |
Alliance S-20A Samarium Cobalt Magnetic Material |
|||
Magnetic Coercive Force, Hc | 16000 Oe | 16000 Oe | Intrinsic |
Alliance S-26A Samarium Cobalt Magnetic Material |
|||
Magnetic Coercive Force, Hc | 16000 Oe | 16000 Oe | Intrinsic |
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
Magnetic Coercive Force, Hc | 16000 Oe | 16000 Oe | Intrinsic |
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
Magnetic Coercive Force, Hc | 16000 Oe | 16000 Oe | Intrinsic |
Alliance S-22A Samarium Cobalt Magnetic Material |