Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 11300 Oe | 11300 Oe | |
Alliance N-38 Neodymium Iron Boron Magnetic Material |
|||
Magnetic Coercive Force, Hc | 11300 Oe | 11300 Oe | |
Alliance N-38H Neodymium Iron Boron Magnetic Material |
|||
Magnetic Coercive Force, Hc | 11300 Oe | 11300 Oe | |
Alliance N-38M Neodymium Iron Boron Magnetic Material |