Polymer Property : Magnetic Coercive Force, Hc = 11000 Oe Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 11000 Oe
11000 Oe
Alliance N-35SH Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 11000 Oe
11000 Oe
Alliance N-35UH Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 11000 Oe
11000 Oe
Alliance N-45 Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 11000 Oe
11000 Oe
Alliance N-45M Neodymium Iron Boron Magnetic Material