Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 1.7 Oe | 1.7 Oe | |
Pacific Sintered Materials F-241-S2 Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE IV, CLASS AAll information provided by Pa.. |
|||
Magnetic Coercive Force, Hc | 1.7 Oe | 1.7 Oe | |
Pacific Sintered Materials F-241-T Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE V, CLASS AAll information provided by Pac.. |
|||
Magnetic Coercive Force, Hc | 1.7 Oe | 1.7 Oe | |
PSM Industries Pacific Sintered Metals Iron F-241-S2 Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type IV, Class AInformation Provided by Pacific Sintered Metals, a d.. |
|||
Magnetic Coercive Force, Hc | 1.7 Oe | 1.7 Oe | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type V, Class AInformation Provided by Pacific Sintered Metals, a di.. |