Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 20200 V | 20200 V | 1hr 120C; ASTM D149 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Dielectric Breakdown | 20200 V | 20200 V | 1hr 94C; ASTM D149 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |