Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 1000 V @Temperature 90.0 °C |
>= 1000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts. Better mechanical properties and poorer electrical properties than type PF CC 204.Information .. |
|||
Dielectric Breakdown | >= 1000 V @Temperature 90.0 °C |
>= 1000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical applications (coarse weave: >130 g/m2, =30 threads/cm). Better mechanical properties and poorer electrical properties than type PF CC 202.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 1000 V | >= 1000 V | Standard condition; ASTM D1000 |
3M Temflex™ 1700 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape 1700 is a good quality, economical general purpose vinyl insulating tape. It has excellent resistance to: abrasion, moisture, alkalies, acid, copper corrosion and vary.. |
|||
Dielectric Breakdown | >= 1000 V | >= 1000 V | Standard condition; ASTM D1000 |
3M Temflex™ 1776 Vinyl Electrical Tape 3M™ Temflex™ Vinyl Electrical Tape 1776 is a good quality, economical, general-purpose vinyl insulating tape, manufactured in the USA. It has excellent resistance to abrasion, moisture, alkalies, .. |