Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 5200 V | 5200 V | Testing Results |
CEN® Electronic Material CS Polyimide Tape CEN® CS polyimide tape is made of CEN® CN polyimide film coated with a high performance silicone adhesive. The tape shows excellent dielectric and insulation properties, high heat resistant, excel.. |