Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 5000 V | 5000 V | Dielectric Strength |
Dielectric Polymers NT-711 Electrical/Mechanical Tape
(discontinued **) High temperature acrylic adhesive with polyester film backing.Features: High temperature shear propertiesSolvent resistantTemperature class: 266°FInsulation resistance: > 1x106 M?Electrolytic corro.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® 2915-10 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M60 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M64 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M69 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M705 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M706 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M716 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M717 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M730 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M741 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M765 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M788 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M797 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M803 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M815 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M824 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M827 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M897 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M97 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® SG03-05(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® SG05-05(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® SG06-05(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M50 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M52 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M56 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Dielectric Breakdown | 5000 V | 5000 V | Standards |
CEN® Electronic Material CS Polyimide Tape CEN® CS polyimide tape is made of CEN® CN polyimide film coated with a high performance silicone adhesive. The tape shows excellent dielectric and insulation properties, high heat resistant, excel.. |
|||
Dielectric Breakdown | >= 5000 V | >= 5000 V | Withstand Voltage AC V |
Fujipoly Industries FLAT-5TV-20-1 silicone rubber fusible tape Information provided by Fujipoly Industries |
|||
Dielectric Breakdown | 5000 V | 5000 V | |
Saint-Gobain CHR® M54 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |