Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 18000 V | 18000 V | |
Saint-Gobain CHR® 2255-6 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | 18000 V | 18000 V | |
Saint-Gobain CHR® TH Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | 18000 V | 18000 V | 1hr 82C; ASTM D149 |
Plenco 3356 Phenolic, Granular, Compression Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Dielectric Breakdown | >= 18000 V | >= 18000 V | IEC 626 |
Dr. D. Mueller Flexiso® DMD FI 14010 00360 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00360 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |