Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 5.00e+11 ohm @Thickness >=3.00 mm |
5.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Insulation Resistance | 5.00e+11 ohm @Thickness >=3.00 mm |
5.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Insulation Resistance | 5.00e+11 ohm @Thickness >=3.00 mm |
5.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Insulation Resistance | 5.00e+11 ohm @Thickness >=3.00 mm |
5.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |
|||
Insulation Resistance | 5.00e+11 ohm @Thickness >=3.00 mm |
5.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |
|||
Insulation Resistance | 5.00e+11 ohm @Thickness >=3.00 mm |
5.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |