Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 5.00e+10 ohm | 5.00e+10 ohm | Wet; 24 hours in water; IEC 167 |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
Insulation Resistance | 5.00e+10 ohm | 5.00e+10 ohm | Wet; 24 hours in water; IEC 167 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Insulation Resistance | >= 5.00e+10 ohm | >= 5.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Insulation Resistance | >= 5.00e+10 ohm | >= 5.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Insulation Resistance | >= 5.00e+10 ohm | >= 5.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Insulation Resistance | >= 5.00e+10 ohm | >= 5.00e+10 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |