Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 2.00e+14 ohm | 2.00e+14 ohm | Insulation Resistance; MIL-I-46058C |
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Insulation Resistance | 2.00e+14 ohm | 2.00e+14 ohm | Insulation Resistance; MIL-I-46058C |
Humiseal 1A27LSE Urethane Conformal Coating Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C).. |
|||
Insulation Resistance | 2.00e+14 ohm | 2.00e+14 ohm | Insulation Resistance; MIL-I-46058C |
Humiseal 1A33 Urethane Conformal Coating Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Insulation Resistance | 2.00e+14 ohm | 2.00e+14 ohm | Insulation Resistance; MIL-I-46058C |
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |