Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | >= 1.50e+8 ohm @Diameter 8.00 - 10.0 mm |
>= 1.50e+8 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe SI GC 41 Woven Glass Cloth Reinforced Silicone Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe. |
|||
Insulation Resistance | >= 1.50e+8 ohm @Diameter 8.00 - 10.0 mm |
>= 1.50e+8 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe EP GC 42 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at elevated temperatures. Very good stability of electrical properties when exposed to high relative .. |