Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1000 - 1.00e+14 ohm | 1000 - 1.00e+14 ohm | Average value: 2.55e+13 ohm Grade Count:4 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Insulation Resistance | 2.00e+7 - 1.00e+14 ohm | 2.00e+7 - 1.00e+14 ohm | Average value: 1.01e+13 ohm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Insulation Resistance | 1.00e+11 - 1.00e+14 ohm | 1.00e+11 - 1.00e+14 ohm | Average value: 2.19e+13 ohm Grade Count:3 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Insulation Resistance | 1.00e+10 - 1.00e+14 ohm | 1.00e+10 - 1.00e+14 ohm | Average value: 4.50e+12 ohm Grade Count:28 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Insulation Resistance | 10.0 - 1.00e+14 ohm | 10.0 - 1.00e+14 ohm | Average value: 4.13e+12 ohm Grade Count:25 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Insulation Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | Dry; IEC 167 |
Vyncolit X655 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask.. |
|||
Insulation Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | Dry; IEC 167 |
Vyncolit X680 Novolac Phenolic Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t.. |
|||
Insulation Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | Dry; IEC 167 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |