Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | >= 5.00e+8 ohm | >= 5.00e+8 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe UP GM 201 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature.Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+8 ohm | >= 5.00e+8 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid.. |
|||
Insulation Resistance | >= 5.00e+8 ohm | >= 5.00e+8 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+8 ohm | >= 5.00e+8 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided .. |
|||
Insulation Resistance | >= 5.00e+8 ohm | >= 5.00e+8 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |