Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 2.00e+7 - 1.00e+14 ohm | 2.00e+7 - 1.00e+14 ohm | Average value: 1.01e+13 ohm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Insulation Resistance | >= 2.00e+7 ohm | >= 2.00e+7 ohm | Gap = 0.25 mm |
Fujipoly Industries FG-S Connector Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre.. |
|||
Insulation Resistance | >= 2.00e+7 ohm | >= 2.00e+7 ohm | Gap = 0.25 mm |
Fujipoly Industries FG-S Fine Connector Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre.. |
|||
Insulation Resistance | >= 2.00e+7 ohm @Diameter 8.00 - 10.0 mm |
>= 2.00e+7 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe PF CC 21 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Fine weave (>30 threads per cm).Information provided by Hippe. |
|||
Insulation Resistance | >= 2.00e+7 ohm @Diameter 8.00 - 10.0 mm |
>= 2.00e+7 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe PF GC 21 Woven Glass Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Very high mechanical strength at moderate temperatures.Information provided by Hippe. |