Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | >= 2.00e+12 ohm | >= 2.00e+12 ohm | C/96/60/95; ASTM D257 |
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Insulation Resistance | >= 2.00e+12 ohm | >= 2.00e+12 ohm | C/96/60/95; ASTM D257 |
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Insulation Resistance | >= 2.00e+12 ohm | >= 2.00e+12 ohm | C/96/60/95; ASTM D257 |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Insulation Resistance | >= 2.00e+12 ohm | >= 2.00e+12 ohm | C/96/60/95; ASTM D257 |
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Insulation Resistance | >= 2.00e+12 ohm | >= 2.00e+12 ohm | C/96/60/95; ASTM D257 |
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Insulation Resistance | 2.00e+12 ohm | 2.00e+12 ohm | Testing Results |
CEN® Electronic Material CS Polyimide Tape CEN® CS polyimide tape is made of CEN® CN polyimide film coated with a high performance silicone adhesive. The tape shows excellent dielectric and insulation properties, high heat resistant, excel.. |