Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.45e+14 ohm | 1.45e+14 ohm | ASTM D-257 |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |