Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 28.0 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 711 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
Short Time; ASTM D149 |
DuPont Performance Polymers Rynite® RE5231 BK533 PET
(Unverified Data**) Rynite® RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 0.800 mm |
711 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 0.800 mm |
711 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 0.800 mm |
711 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 0.800 mm |
711 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 0.800 mm |
711 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 2.00 mm |
711 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 2.00 mm |
711 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 2.00 mm |
711 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 2.00 mm, Temperature 90.0 °C |
711 kV/in @Thickness 0.0787 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |