Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 101R PC (Europe-Africa-Middle East) LEXAN 101R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 101R is available in transparent, translucent and opaque colours. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 161R PC (Europe-Africa-Middle East) LEXAN 161R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 161R is available in transparent, translucent and opaque colours. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 244R PC (Europe-Africa-Middle East) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also US FDA food contact compliant available in limited colorsThis dat.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® IR2210 PC (Europe-Africa-Middle East) IR2210 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics Lexan® PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East) LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East) LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1003R PC PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was .. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1003R PC (Europe-Africa-Middle East) PC1003R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800R PC (Asia Pacific) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC1803R PC PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC1803R PC (Asia Pacific) PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2203R PC PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2203R PC (Asia Pacific) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC1500 PC (Asia Pacific) PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC2200 PC PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |