Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 24.6 kV/mm @Thickness 1.57 mm |
625 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP320E Cotton Fabric Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500†|
|||
Dielectric Strength | 24.6 kV/mm @Thickness 1.57 mm |
625 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |