Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.5 kV/mm @Thickness 1.00 mm |
419 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 133R PC (Europe-Africa-Middle East) LEXAN 133R is the highest viscosity, UV stabilized, release containing, linear polycarbonate grade. Suitable for injection molding and extrusion processes. Available in transparent and multiple colo.. |
|||
Dielectric Strength | 16.5 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
419 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
500 V/s, in oil; Short Time; ASTM D149 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |