Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.7 kV/mm @Thickness 1.57 mm |
400 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 1.57 mm |
400 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |