Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 124R PC UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP2R PC Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP4R PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP4R PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS2R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HF1140 PC Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP2NR PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Dielectric Strength | 14.9 kV/mm @Frequency 60.0 Hz |
378 kV/in @Frequency 60.0 Hz |
short time, wet; ASTM D149 |
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1960B-1 is a mineral and short fiberglass filled epoxy compound, formulated for the encapsulation of passive electronic devices.Information provided by Sumitomo Bak North America, Inc. |